| The excellent dispersion properties of this
admixture both for ready mix and site mix concrete allow the
production of very high, early and high strength concrete
with minimal voids.
Can be placed and compacted in congested reinforcement.
Increases the Compressive Strength of the Concrete upto
42.0MPa
Reduces Water Absorption 78%
Setting time is within permissible limit of ISI Standards.
Long retention of the slump
Improved surface finish
High workability without segregation or bleeding
Less vibration required
|